FIELD: chemistry.
SUBSTANCE: additive is obtained by reacting C10-C12 α-olefins with sulphur at temperature of 130-140°C in the presence of 0.5-2.0 wt % catalyst - calcium thio-bis(alkylphenolate).
EFFECT: high output of the sulphur-containing additive and simple process.
4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING SULPHUR-CONTAINING ADDITIVE | 2009 |
|
RU2423413C2 |
METHOD OF PREPARING SULFUR-CONTAINING ADDITIVES | 2000 |
|
RU2181137C1 |
ANTISCORING AND ANTIWEAR OIL ADDITIVES OPERATING AT HIGH PRESSURE | 2008 |
|
RU2382816C1 |
ANTISCORING AND ANTIWEAR ADDITIVES FOR OIL WORKING UNDER HIGH PRESSURE | 2008 |
|
RU2434936C2 |
ANTISCORING AND ANTIWEAR ADDITIVES FOR OIL WORKING AT HIGH PRESSURE | 2009 |
|
RU2418042C2 |
METHOD OF PREPARING SULFUR-CONTAINING ADDITIVES | 1999 |
|
RU2168536C2 |
ANTICORROSION ADDITIVE FOR LUBRICATING OIL | 2010 |
|
RU2455346C2 |
METHOD OF PREPARING SULFUR-CONTAINING ADDITIVES | 1998 |
|
RU2148617C1 |
PROCESS LUBRICANT FOR METAL COLD DIE FORGING | 2008 |
|
RU2400532C2 |
METHOD OF PREPARING SULFUR- AND NITROGEN-CONTAINING ADDITIVES | 2003 |
|
RU2243253C1 |
Authors
Dates
2012-12-10—Published
2010-04-14—Filed