FIELD: metallurgy.
SUBSTANCE: method involves production of a semi-finished product in a steel making unit, steel tapping to a ladle, cutoff during furnace slag tapping, addition to the ladle at tapping of solid slag-forming mixture, and out-of-furnace treatment at a furnace-ladle unit. At tapping, solid slag-forming mixture in quantity of 2.0-2.7 kg/t consisting of lime 75-80 wt % and fluorite-sellaite concentrate 20-25 wt % is added to the ladle; treatment is performed at the furnace-ladle unit during 45-75 minutes; at that, in order to complete metal desulphurisation, the same solid slag-forming mixture in quantity of 0.3-0.6 kg/t consisting of lime 75-80 wt % and fluorite-sellaite concentrate 20-25 wt % is added to the ladle; steel is blown with argon during treatment through bottom porous tuyere blocks with flow rate of 20-50 m3/h.
EFFECT: invention allows increasing metal desulphurisation degree and reducing slag thinner consumption.
1 tbl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
SOLID SLAG-FORMING MIXTURE TO REFINE STEEL | 2010 |
|
RU2450059C1 |
METHOD OF OUT-OF-FURNACE TREATMENT OF STEEL IN LADLE | 2020 |
|
RU2735697C1 |
METHOD OF PRODUCING STEEL WITH SPECIFIED LIMIT ON SULPHUR CONTENT | 2023 |
|
RU2816888C1 |
LOW-SILICON STEEL PRODUCTION METHOD | 2023 |
|
RU2818526C1 |
METHOD FOR OFF-FURNACE STEEL TREATMENT | 2015 |
|
RU2607877C2 |
METHOD FOR STEEL AFTERTREATMENT | 1996 |
|
RU2108400C1 |
METHOD OF PRODUCTION OF ELECTRIC STEEL | 2008 |
|
RU2366724C1 |
METHOD OF DRY STEEL PRODUCTION | 2013 |
|
RU2533263C1 |
STEELMAKING PROCESS | 0 |
|
SU1747502A1 |
METHOD OF RECEIVING OF HIGH-CARBON STEEL OF CORD QUALIT | 2008 |
|
RU2378391C1 |
Authors
Dates
2013-04-20—Published
2012-03-13—Filed