FIELD: process engineering.
SUBSTANCE: invention relates to laser engineering, particularly, to laser gyroscopy. Metal part is placed on glass ceramics block. Bulge is made between surfaces to be bonded together by straying powder at angle of 75-90 degrees to bond surface. Block with part are placed in kiln heated to 400-450°C and exposed for, at least, one hour. Then, its is cooled to room temperature at the rate of, at least, 5 °C/min.
EFFECT: higher precision and safety of annular laser gyroscope.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SEALING GLASS-CERAMIC WITH METAL DETAIL | 2016 |
|
RU2623386C1 |
METHOD OF HERMETICALLY JOINING GLASS CERAMICS WITH METALLIC PART | 2003 |
|
RU2238249C2 |
METHOD OF DECREASING OF MAGNETIC DRIFT OF ZEEMAN LASER GYROSCOPES | 2014 |
|
RU2550376C1 |
METHOD OF INCREASING RELIABILITY OF RING LASER GYROSCOPES | 2016 |
|
RU2638566C2 |
LASER GYRO RING RESONATOR | 2017 |
|
RU2660290C1 |
LASER APPARATUS FOR THERMAL TREATMENT OF BULK GETTERS | 2020 |
|
RU2751404C1 |
ION-PLASMA CLEANING OF GAS LASER RESONATOR INNER SURFACE | 2014 |
|
RU2562615C1 |
METHOD TO MEASURE ANGULAR MOVEMENTS BY LASER GYROSCOPE | 2013 |
|
RU2525648C1 |
METHOD FOR PRODUCING SOLID-STATE LASER PUMP | 2002 |
|
RU2225061C1 |
METHOD OF MEASURING THE SURFACE PROFILE OF OPTICAL PARTS USING LASER PHASE-SHIFTING INTERFEROMETRY | 2019 |
|
RU2722631C1 |
Authors
Dates
2013-06-20—Published
2012-04-25—Filed