FIELD: electricity.
SUBSTANCE: steel wire is aluminised during 1-3 cycles, and each cycle consists of heating of steel wire up to temperature of 900°C in shielding atmosphere to the depth of aluminium to steel, submerging to the bath with molten aluminium and intensive cooling up temperature of 550°C after treatment by molten aluminium and the latter is covered by a layer of molten cryolite in order to prevent oxidation of molten aluminium.
EFFECT: corrosion resistivity of the wire.
Title | Year | Author | Number |
---|---|---|---|
METHODS OF CONTACT STEEL ALUMINIUM WIRE PRODUCTION | 2014 |
|
RU2594756C2 |
METHOD OF INCREASING RESISTANCE OF STEEL PIPELINES AGAINST CORROSION BY ALUMINIZING | 2014 |
|
RU2590738C1 |
METHOD OF MANUFACTURING HIGH-STRENGTH STEEL-ALUMINIUM WIRE | 0 |
|
SU1117325A2 |
PROCEDURE FOR ALLOYING STEEL WITH ALUMINIUM | 2009 |
|
RU2431696C2 |
METHOD OF SPOT ELECTROCONTACT WELDING OF ALUMINIUM AND ITS ALLOYS | 2008 |
|
RU2374049C1 |
METHOD OF MAKING HIGH-STRENGTH STEEL-ALUMINIUM WIRE | 0 |
|
SU881136A1 |
METHOD OF MAINLY STEEL ALUMINIUM WIRE MANUFACTURING | 2007 |
|
RU2351486C2 |
METHOD OF PRODUCING STEEL-ALUMINIUM WIRE | 0 |
|
SU1066694A1 |
METHOD FOR PRODUCING HEAT-RESISTANT COATING | 2023 |
|
RU2807248C1 |
NON-INSULATED STEEL-ALUMINUM HIGH-TEMPERATURE HIGH-STRENGTH WIRE | 2019 |
|
RU2706957C1 |
Authors
Dates
2013-08-20—Published
2010-03-17—Filed