FIELD: power engineering.
SUBSTANCE: composition contains lithium fluoride, chloride, metavanadate, molybdate and potassium chloride at the following ratio of components, wt %: lithium fluoride 2.0…2.2; lithium chloride 36.2…36.6; lithium metavanadate 3.1…8.7; lithium molybdate 15.0…16.4; potassium chloride 37.7…42.1.
EFFECT: provision of mixture operability in a heat accumulator, possibility to use the proposed mixture as coolant with temperature range expansion in comparison with the available ones.
3 ex
Title | Year | Author | Number |
---|---|---|---|
LOW-MELTING HEAT STORAGE SALT MIXTURE | 2022 |
|
RU2799874C1 |
LOW-MELTING HEAT STORAGE SALT MIXTURE | 2023 |
|
RU2813183C1 |
HEAT-STORAGE COMPOSITION | 2004 |
|
RU2272823C1 |
HEAT CARRIER FROM HALIDES OF ALKALI METALS | 2022 |
|
RU2817998C2 |
HEAT-ACCUMULATING COMPOSITION | 2023 |
|
RU2822273C1 |
ELECTROLYTE FOR CHEMICAL CURRENT SOURCE | 2011 |
|
RU2484556C2 |
MELTABLE ELECTROLYTE FOR CHEMICAL SOURCE OF CURRENT | 2013 |
|
RU2555369C1 |
HEAT-ACCUMULATING MIXTURE OF LITHIUM, SODIUM AND CALCIUM HALIDES | 2023 |
|
RU2819041C1 |
HEAT-STORAGE COMPOSITION | 2004 |
|
RU2272822C1 |
HEAT-ACCUMULATING COMPOSITION | 2015 |
|
RU2605989C1 |
Authors
Dates
2013-09-10—Published
2012-03-11—Filed