FIELD: metallurgy.
SUBSTANCE: coating first layer of refractory compound is applied. Then, second layer with grain size of 40-60 nm is applied. Now, magnetic-pulse processing if carried out for 15-20 minutes.
EFFECT: higher adhesion and crack growth resistance.
1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| MULTILAYER COATING ON HARD ALLOY TOOL FOR TREATMENT OF TITANIUM ALLOYS AND PROCEDURE FOR ITS FABRICATION | 2009 |
|
RU2415198C1 |
| CEMENTED METAL TIP AND METHOD OF ITS MANUFACTURE | 1995 |
|
RU2104826C1 |
| METHOD TO APPLY COMBINED PVD/CVD/PVD COATINGS ONTO CUTTING HARD-ALLOY TOOL | 2011 |
|
RU2468124C1 |
| PROCEDURE FOR COATING ITEMS OUT OF HARD ALLOYS | 2009 |
|
RU2415966C1 |
| CUTTING PLATE MANUFACTURING METHOD | 2011 |
|
RU2485208C2 |
| PROCESS OF HARDENING OF HARD-ALLOY CUTTING TOOL | 1999 |
|
RU2167216C1 |
| METHOD OF PRODUCING ION-PLASMA VACUUM-ARC CERAMETALLIC Ti-Ni COATING FOR CARBIDE CUTTING TOOL OF EXPANDED USE | 2015 |
|
RU2613837C1 |
| METHOD OF PRODUCING SUPERHARD COMPOSITE MATERIAL FOR CUTTING TOOLS | 2023 |
|
RU2829867C1 |
| METHOD OF OBTAINING MULTI-LAYERED COATING FOR CUTTING INSTRUMENT | 2013 |
|
RU2532741C1 |
| METHOD FOR PRODUCING HARD-ALLOY LAMINATED COMPOSITE MATERIAL | 1988 |
|
SU1526046A1 |
Authors
Dates
2013-09-27—Published
2012-01-23—Filed