FIELD: metallurgy.
SUBSTANCE: precleaning of tool surface and subsequent vacuum-arc coating deposition are carried out in the reaction gas-nitrogen during evaporation of cathodes containing titanium and nickel. Coating deposition is carried out during evaporation of cathodes made of VT1 and Ti-Ni (50 at titanium alloys.% Ni) in the arc current which evaporates cathode from titanium, 120 A and in the arc current which evaporates the cathode from Ti-Ni alloy, 90-110 A, and 100-120 V negative bias voltage fed to the carbide cutting tool. These deposition parameters and used cathode materials allow to implement 3.5-8% (at.) nickel content in the coatings.
EFFECT: increased durability of the carbide cutting tool; expansion of its use both at continuous and interrupted cutting operations; increased turning speed of the processed materials.
9 dwg, 7 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF ION-PLASMA VACUUM-ARC CERAMIC-METAL COATING TiN-Cu FOR CARBIDE CUTTING TOOL WITH EXTENDED APPLICATION SCOPE | 2014 |
|
RU2573845C1 |
METHOD TO APPLY COMBINED PVD/CVD/PVD COATINGS ONTO CUTTING HARD-ALLOY TOOL | 2011 |
|
RU2468124C1 |
METHOD OF OBTAINING ADAPTIVE WEAR-RESISTANT Ti-Al-Mo-N COATING FOR PROTECTING FROM WEARING IN VARIABLE FREQUENCY CONDITIONS | 2016 |
|
RU2644094C1 |
PROCEDURE FOR APPLICATION OF COATING ON HARDMETAL | 2015 |
|
RU2615941C1 |
METHOD OF VACUUM-ION-PLASMA DEPOSITION OF MULTILAYER WEAR-PROOF COATING FOR CUTTING TOOL | 2011 |
|
RU2478138C1 |
PROCEDURE FOR PRODUCTION OF WEAR-RESISTANT COATING FOR CUTTING TOOL | 2009 |
|
RU2423547C2 |
METHOD FOR HYBRID OBTAINING OF WEAR-RESISTANT COATING ON CUTTING TOOL | 2011 |
|
RU2485210C2 |
METHOD OF DEPOSITING AMORPHOUS-CRYSTALLINE COATING ON METAL CUTTING TOOL | 2019 |
|
RU2699700C1 |
METHOD FOR WEAR RESISTANCE COATING APPLICATION ON CUTTING TOOL | 2003 |
|
RU2250931C1 |
METHOD FOR APPLYING LAMINATE COATING ON CUTTING TOOL | 2004 |
|
RU2260631C1 |
Authors
Dates
2017-03-21—Published
2015-12-03—Filed