FIELD: chemistry.
SUBSTANCE: invention relates to production of pellet powder for small arms. After completion of the process of dispersing powder lacquer on spherical particles at mixture temperature in the reactor of 68…70°C, sodium sulphate (NazSO4) is fed into the reactor in amount of 0.6…1.5 wt % with respect to water and the process of distilling the solvent is started immediately.
EFFECT: invention provides stable porosity of powder elements of pellet powder.
3 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF SPHERICAL POWDER FOR SPORT HUNTING CARTRIDGE 30 CARBINE (7,62×33) | 2010 |
|
RU2452720C2 |
METHOD OF PRODUCING PELLET POWDER FOR SMALL ARM CARTRIDGES | 2011 |
|
RU2495012C2 |
METHOD OF PRODUCING SPHERICAL POWDER FOR 5,6 MM-SPORTING CALIBER CARTRIDGES WITH ANNULAR IGNITION | 2010 |
|
RU2451652C2 |
METHOD OF PRODUCING PYROXYLINE PELLET POWDER FOR 7,62 MM SPORT CARTRIDGE | 2015 |
|
RU2597391C2 |
METHOD TO PRODUCE SPHERICAL PYROXILIC POWDER FOR 9 mm PISTOL CARTRIDGE | 2010 |
|
RU2448078C2 |
PRODUCTION OF GUN-COTTON SPHERICAL POWDER FOR 7,62 mm SPORTING ROUND | 2013 |
|
RU2527781C1 |
METHOD OF PRODUCTION OF SPHERICAL POWDER FOR SHOT CARTRIDGES FOR SMOOTH-BORE SPORTS AND HUNTING WEAPONS OF 12, 16 AND 20 CALIBRE | 2012 |
|
RU2522642C2 |
METHOD OF PRODUCING HIGH-DENSITY PELLET POWDER | 2016 |
|
RU2655362C2 |
METHOD OF PREPARING PELLET POWDER WITH PARTICLE DIAMETER OF UP TO 2,5 MM | 2009 |
|
RU2421434C2 |
METHOD OF PRODUCING PELLET POWDER FOR CARTRIDGES OF SPORTS AND HUNTING WEAPONS | 2011 |
|
RU2495011C2 |
Authors
Dates
2013-10-10—Published
2011-12-14—Filed