FIELD: metallurgy.
SUBSTANCE: method for steel pouring to a steel-pouring ladle involves pre-deoxidation and alloying with manganese-containing ferroalloys, out-of-furnace metal treatment is performed at a circulation steel vacuumising plant; at that, negative pressure is set in a vacuum chamber for not more than 10 mbar and argon consumption for mixing is 0.8 to 1.1 l/(t*min). After that, final deoxidation and metal alloying in the vacuum chamber is performed with aluminium shot in the quantity of 1.5…2.5 kg/t in terms of obtaining the required content of aluminium in metal. At that, total duration of vacuumising is set from 10 to 15 minutes.
EFFECT: invention allows maximum elimination of non-metallic inclusions, reduction of aluminium consumption and stabilisation of metal pouring process owing to improving poured steel quality.
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR PRODUCTION OF LOW CARBON STEEL | 2010 |
|
RU2437942C1 |
METHOD FOR PRODUCING CORROSION-RESISTANT TITANIUM STEEL | 2020 |
|
RU2786736C2 |
METHOD OF PRODUCING STEEL WITH SPECIFIED LIMIT ON SULPHUR CONTENT | 2023 |
|
RU2816888C1 |
METHOD FOR MAKING HIGH QUALITY STEEL | 1998 |
|
RU2139943C1 |
METHOD OF MAKING STEEL FOR METAL CORD | 2003 |
|
RU2265064C2 |
METHOD OF LOW-CARBON STEEL DEOXIDATION | 2012 |
|
RU2514125C1 |
METHOD OF PRODUCING OF LOW ALLOYED PIPE STEEL | 2014 |
|
RU2574529C1 |
LOW-SILICON STEEL PRODUCTION METHOD | 2023 |
|
RU2818526C1 |
METHOD FOR PRODUCTION OF SUPER PURE ALUMINUM DEOXIDISED FOR PRODUCTION OF HIGH-QUALITY METAL PRODUCTS | 2019 |
|
RU2740949C1 |
METHOD FOR PRODUCTION OF LOW-ALLOYED PIPE STEEL | 2012 |
|
RU2487171C1 |
Authors
Dates
2013-10-10—Published
2012-05-14—Filed