FIELD: metallurgy.
SUBSTANCE: in compliance with this method, hard slag-forming mix (HSFM), aluminium and ferromanganese are introduced to steel teeming ladle from the converter. Note here that during metal tapping into teeming ladle secondary aluminium ingots and carbon ferromanganese are used as deoxidisers. Note here that in case the ladle is filled for its 1/5-1/4-volume 0.8…1.0 kg/t of secondary aluminium ingots are introduced. Note that the ladle is filled for its 1/3-1/2-volume 1.5…3.5 kg/t of carbon ferromanganese are added. Note here that in case the ladle is filled for its 1/2-2/3-volume 1.5…2.0 kg/t of secondary aluminium ingots and HSFM are introduced. Note also that during the metal tapping from converter, metal is blown with argon via ladle bottom plugs at intensity of 0.2…0.5 l/(t*min) for 5…8 min.
EFFECT: better recovery of aluminium and ferroalloys, stabilised teeming, better steel quality.
Title | Year | Author | Number |
---|---|---|---|
METHOD OF LADLE TREATMENT OF ALLOYED STEELS | 2016 |
|
RU2637194C1 |
METHOD FOR PRODUCTION OF LOW-ALLOYED PIPE STEEL | 2012 |
|
RU2487171C1 |
METHOD OF PRODUCING STEEL WITH SPECIFIED LIMIT ON SULPHUR CONTENT | 2023 |
|
RU2816888C1 |
LOW-CARBON STEEL MAKING METHOD | 2012 |
|
RU2495139C1 |
METHOD OF MELTING LOW-CARBON TITANIUM-CONTAINING STEEL | 2003 |
|
RU2243269C1 |
METHOD OF PRODUCTION OF THE CARBON STEEL | 2006 |
|
RU2304622C1 |
DEOXIDATION METHOD OF METAL FOR COLD FORGING | 2008 |
|
RU2377315C1 |
METHOD OF PRODUCING OF LOW ALLOYED PIPE STEEL | 2014 |
|
RU2574529C1 |
METHOD OF MAKING STEEL FOR METAL CORD | 2003 |
|
RU2265064C2 |
LOW-SILICON STEEL PRODUCTION METHOD | 2023 |
|
RU2818526C1 |
Authors
Dates
2014-04-27—Published
2012-11-30—Filed