FIELD: chemistry.
SUBSTANCE: invention relates to material science. The method of producing a polytetrafluoroethylene-based antifrictional polymer composite involves preliminary physical and chemical treatment of ultrafine detonation diamond powder, mechanical dispersion of the mixture of powdered polytetrafluoroethylene and ultrafine detonation diamond, pressing and sintering the composite in an inert medium. Physical and chemical treatment of the ultrafine detonation diamond powder involves heating therein in an inert medium at temperature of 700-800°C for 20-30 minutes with continuous removal of gaseous thermal desorption products until removal of oxygen-containing surface groups, characterised by an absorption band in infrared spectra with a maximum in the wave number range of 1730 - 1850 cm-1.
EFFECT: invention improves tribological properties of the composite and uniformity of its properties on a sample volume.
3 cl, 5 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING HIGH-MOLECULAR WEIGHT POLYTETRAFLUOROETHYLENE | 2014 |
|
RU2601000C2 |
ACCUMULATIVE ANTIFRICTION AND SEALING MATERIAL BASED ON POLYTETRAFLUOROETHYLENE | 2011 |
|
RU2467034C1 |
METHOD OF FUNCTIONALISATION OF DETONATION NANODIAMOND SURFACE | 2010 |
|
RU2473464C2 |
METHOD FOR FUNCTIONALIZATION OF SURFACE OF DETONATION NANODIAMONDS | 2015 |
|
RU2676975C2 |
NANOCOMPOSITE POLYTETRAFLUOROETHYLENE-BASED CONSTRUCTION MATERIAL | 2011 |
|
RU2467033C1 |
METHOD OF MAKING DIAMOND-CARBON NANOPARTICLES | 2008 |
|
RU2384523C2 |
COMPOSITION FOR OBTAINING COATING WITH IMPROVED TRIBOTECHNICAL PROPERTIES AND COATING METHOD | 2012 |
|
RU2495893C1 |
METHOD FOR SELECTIVE PURIFICATION OF DETONATION NANODIAMONDS | 2010 |
|
RU2463249C2 |
ANTIFRICTION POLYMER COMPOSITION WITH SEALING CAPABILITY | 1994 |
|
RU2114874C1 |
GREASE | 2009 |
|
RU2395563C1 |
Authors
Dates
2013-10-20—Published
2011-08-24—Filed