FIELD: chemistry.
SUBSTANCE: anticorrosion pigment is produced from electric furnace wastes from foundry production - aspiration fines, containing, wt %: Fe2O3 63.9-70.0, FeO 7.0-11.32, SiO2 8.9-16, Al2O3 1.45-3.12. The aspiration fines are mixed in dry form with dolomite powder containing magnesium and calcium bicarbonate in amount of 80-95 wt %, with the ratio of aspiration fines to dolomite powder of 60-40:40-60 wt %, respectively. The obtained mixture is calcined for 3-5 hours at temperature of 700-800°C.
EFFECT: invention simplifies production of the anticorrosion pigment and lowers the calcining temperature.
1 tbl, 28 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING ANTICORROSION PIGMENT | 2014 |
|
RU2570455C2 |
METHOD OF PREPARING ANTICORROSION PIGMENT | 2008 |
|
RU2391365C2 |
ANTICORROSION PIGMENT FOR PRIMERS AS APPLIED TO METAL | 1999 |
|
RU2169162C2 |
METHOD OF MAKING CHROMATE ANTICORROSIVE PIGMENT | 2007 |
|
RU2382062C2 |
METHOD OF PREPARATION OF THE CATALYST FOR STEAM REFORMING OF OIL AND HYDROCARBON GASES | 2016 |
|
RU2620605C1 |
ANTICORROSIVE PIGMENTS | 2001 |
|
RU2216560C2 |
METHOD FOR PRODUCING ANTI-CORROSION PIGMENT | 2023 |
|
RU2807930C1 |
METHOD OF PRODUCING IRON-CALCIUM PIGMENT | 2010 |
|
RU2451706C1 |
ANTICORROSIVE PIGMENTS | 2004 |
|
RU2256617C1 |
ANTICORROSIVE PIGMENT | 2006 |
|
RU2302437C1 |
Authors
Dates
2014-01-27—Published
2012-07-20—Filed