FIELD: chemistry.
SUBSTANCE: brown coal is crushed to -50+25 mm pieces, after which the crushed brown coal is subjected to pyrolysis to obtain carbonated coal. The carbonated coal is crushed to -2.5+0.5 mm pieces and subjected to heat treatment with steam to obtain activated carbonated coal. Treatment with dichloroethane is then carried out, followed by treatment with oleum at 70-90°C.
EFFECT: high activity of the sorbent with respect to mercury ions owing to higher degree of sulphonation.
5 cl, 6 tbl, 25 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING SULPHOCATIONITE FROM COAL | 2023 |
|
RU2823758C1 |
SULFONATED COAL PRODUCTION PROCESS | 2002 |
|
RU2213693C1 |
METHOD FOR PREPARING SORBENT | 1992 |
|
RU2049055C1 |
METHOD FOR PREPARATION OF PROTEINOUS SORBENT | 0 |
|
SU1680715A1 |
METHOD OF PRODUCING SELECTIVE SORBENT | 2015 |
|
RU2589484C1 |
PROCESS FOR PREPARING SULFONATED STYRENE-DIVINYLBENZENE COPOLYMER | 0 |
|
SU1060627A1 |
METHOD OF SULFONATED COAL PRODUCING | 1992 |
|
RU2010000C1 |
METHOD OF OBTAINING CATIONITE FOR SOFTENING AND DESALINATING WATER | 0 |
|
SU1574593A1 |
METHOD OF PRODUCING SULPHUR-CONTAINING SORBENTS FOR REMOVING HEAVY METALS FROM WASTE WATER | 2010 |
|
RU2475299C2 |
METHOD OF SORPTION PURIFICATION OF WATER FROM AMMONIUM NITROGEN OF FISH FARMING ENTERPRISES | 2017 |
|
RU2671329C1 |
Authors
Dates
2014-02-27—Published
2012-07-25—Filed