FIELD: chemical technology. SUBSTANCE: woody fiber of flax is treated within 15-20 min by 10-12 M solution of sulfuric acid, at weight ratio 1: 5-6, the process being carried out at 150-155 C. EFFECT: improves efficiency of method. 3 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD FOR PRODUCING SORBENT FROM FLAX PROCESSING WASTE | 2021 |
|
RU2805033C2 |
| METHOD OF PRODUCING CARBOXYMETHYLATED LIGNOCARBOHYDRATE MATERIAL | 2008 |
|
RU2374264C1 |
| METHOD OF MAKING SORBENT | 2012 |
|
RU2508248C1 |
| METHOD FOR OBTAINING SORBENT FOR PURIFYING WASTEWATER FROM MULTICOMPONENT POLLUTANTS | 2017 |
|
RU2644880C1 |
| METHOD OF OBTAINING SORBENT | 2023 |
|
RU2816067C1 |
| COMPLEXING SORBENT, METHOD FOR PREPARATION THEREOF, AND USE | 2004 |
|
RU2270056C2 |
| METHOD OF PURIFICATION OF CARBON SORBENT | 1998 |
|
RU2141450C1 |
| METHOD OF PURIFICATION OF WASTE WATER FROM IONS OF CHROMIUM (III) AND (IV) | 2005 |
|
RU2291113C1 |
| HUMIC PRODUCTION WASTE FOR WASTEWATER TREATMENT | 2023 |
|
RU2832437C1 |
| SORBENT BASED ON KELP FIBER | 2016 |
|
RU2637436C1 |
Authors
Dates
1995-11-27—Published
1992-10-27—Filed