FIELD: chemistry.
SUBSTANCE: cement concrete that self-decomposes in water is made from a mixture containing, wt %: portland cement with limestone 26.0-56.0, high-alumina cement 0.6-2.4, hemihydrate gypsum 3.0-6.0, quartz sand - the balance; hardening water of the mixture with water to solid ratio of 0.1-0.18; a plasticiser can be used.
EFFECT: obtaining self-decomposing concrete with controlled time of full decomposition in water ranging from 2 weeks to 6-9 months.
2 cl, 7 tbl, 18 dwg
Title | Year | Author | Number |
---|---|---|---|
ANCHOR FOR SUBMERSING ANCHORING UNDERWATER RESEARCH HARDWARE AT BOTTOM | 2011 |
|
RU2509676C2 |
METHOD FOR PRODUCTION OF NONCONTRACTING, CORROSION-RESISTANT PORTLANDCEMENT BINDER | 2003 |
|
RU2243945C2 |
ORGANOMINERAL MODIFIER FOR GYPSUM BINDING MATERIALS AND RADIOPROTECTIVE ARTICLES BASED THEREON | 2018 |
|
RU2710647C2 |
METHOD OF PRODUCTION OF BINARY PLASTICIZED PORTLAND CEMENT BINDERS | 2004 |
|
RU2303010C2 |
ORGANOMINERAL MODIFIER FOR GYPSUM COMPOSITIONS AND RADIOPROTECTIVE ARTICLES BASED THEREON | 2018 |
|
RU2710643C2 |
ORGANOMINERAL MODIFIER FOR GYPSUM MIXTURES AND RADIOPROTECTIVE ARTICLES BASED THEREON | 2018 |
|
RU2710245C2 |
DRY COMPOSITION FOR CREATION OF SELF-LEVELLING RAPIDLY HARDENING LIQUID FLOORS | 2013 |
|
RU2540703C2 |
EXPANSION ADMIXTURE BASED ON IRON-CONTAINING PULVERIZED WASTE FOR EXPANDING CEMENT | 2021 |
|
RU2767481C1 |
DRY MIXTURE FOR LEVELING OF VESSELS DECKS | 2018 |
|
RU2689959C1 |
EXPANDING GROUTING MORTAR ( VARIANTS ) | 2001 |
|
RU2222688C2 |
Authors
Dates
2014-03-10—Published
2011-12-29—Filed