FIELD: chemistry.
SUBSTANCE: method of obtaining thermoplastic elastomeric composition is realised by dynamic mixing of polyethylene with chlorosulfonated polyethylene. In the process of dynamic mixing of polymers in composition introduced is e- caprolactam in quantity 5-10 wt.p. per 100 wt.p. of polymer mixture, which ensures index of composition melt fluidity, determined under load 21.6 kg and temperature 150°C, 7.3-15.1 g/10 min.
EFFECT: obtaining thermoplastic elastomeric composition with improved processability and elasticity, with preservation of resistance to ozone, atmosphere and oil and petrol resistance.
1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PRODUCING THERMOPLASTIC ELASTOMER COMPOSITION | 2012 |
|
RU2497844C1 |
| METHOD OF PRODUCING THERMOPLASTIC ELASTOMERIC COMPOSITION | 2011 |
|
RU2458943C1 |
| THERMOPLASTIC ELASTOMERIC COMPOSITION | 2011 |
|
RU2473574C2 |
| METHOD OF OBTAINING THERMOPLASTIC ELASTOMER COMPOSITION | 2012 |
|
RU2519401C2 |
| THERMOPLASTIC ELASTOMER COMPOSITION BASED ON BLOCK-COPOLYMER OF STYRENE AND CRYSTALLINE POLYMERS AND METHOD OF ITS PREPARATION | 2013 |
|
RU2556638C2 |
| METHOD FOR OBTAINING HEAT-INSULATING MATERIAL, BASED ON WOOD AND THERMOPLASTIC WASTES | 2014 |
|
RU2581047C2 |
| THERMOPLASTIC ELASTOMERIC COMPOSITION BASED ON NATURAL RUBBER AND POLYVINYLCHLORIDE | 2017 |
|
RU2655345C1 |
| WATER-OIL-SWELLING THERMOPLASTIC ELASTOMER COMPOSITION | 2018 |
|
RU2690929C1 |
| METHOD FOR PRODUCING A THERMOPLASTIC ELASTOMER ON THE BASIS OF NATURAL RUBBER AND POLYVINYLCHLORIDE | 2017 |
|
RU2663045C1 |
| ELECTROCONDUCTIVE THERMOPLASTIC ELASTOMER COMPOSITION | 2018 |
|
RU2690806C1 |
Authors
Dates
2014-04-10—Published
2012-12-27—Filed