FIELD: construction.
SUBSTANCE: concrete mix includes portland cement, filler, tempering water and additive - complex solution with pH=4-5 with H4SiO4 sol base, besides, the specified complex solution is prepared at the following ratio of mixture components, wt %: microsilica 0.113-0.227, superplasticiser Relamix type 2 with pH=9±1 0.076-0.15, concentrated hydrochloric or acetic acid, or sulphuric acid 0.011-0.023, water 3.58-7.16 at the following ratio of concrete mix components, wt %: portland cement 22.63-22.68; filler 67.91-68.04; specified additive 3.78-7.56; tempering water 1.9-5.5.
EFFECT: higher strength of concrete during compression and reduced consumption of expensive additives of microsilica and superplasticiser.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHODS OF INCREASING CONCRETE STRENGTH AT COMPRESSION USING NANOSILICA OBTAINED FROM HYDROTHERMAL SOLUTION | 2015 |
|
RU2599739C1 |
NANOMODIFIED CONCRETE AND METHOD FOR PRODUCTION THEREOF | 2013 |
|
RU2559269C2 |
CONCRETE MIXTURE | 2011 |
|
RU2461524C1 |
HIGH-STRENGTH FINE GRAIN CONCRETE | 2016 |
|
RU2641813C2 |
RAW MATERIAL MIXTURE | 2009 |
|
RU2396235C1 |
METHOD TO MAKE CONCRETE MIX | 2009 |
|
RU2416582C1 |
NANO-MODIFIED CEMENT COMPOSITE FOR CONSTRUCTION 3D PRINTING | 2021 |
|
RU2767643C1 |
METHOD FOR MODIFYING CONCRETE WITH COMPLEX ADDITIVE INCLUDING HYDROTHERMAL SIO2 NANOPARTICLES AND MULTILAYER CARBON NANOTUBES | 2020 |
|
RU2750497C1 |
CONCRETE MIX AND METHOD OF PREPARATION OF SUCH MIX | 2006 |
|
RU2307810C1 |
CRUDE MIXTURE FOR PROTECTIVE COATING OF SURFACE OF CARNALLITE ROCK | 2015 |
|
RU2581062C1 |
Authors
Dates
2014-05-20—Published
2012-12-26—Filed