FIELD: metallurgy.
SUBSTANCE: solder contains components at the following ratio in wt %: zirconium - 45-50, beryllium - 2.5-4.5, aluminium - 0.5-1.5, titanium making the rest. Solder represents a flexible band and is produced by super-rapid tempering of the alloy by casting the melt of revolving disc.
EFFECT: higher operating performances, decreased intermetallide interlayers in the weld.
3 cl, 11 dwg, 1 ex
Title | Year | Author | Number |
---|---|---|---|
AMORPHOUS COPPER-BASED STRIP SOLDER | 2011 |
|
RU2464143C1 |
METHOD FOR OBTAINING MOLYBDENUM AND GRAPHITE BRAZED JOINT | 2016 |
|
RU2646300C2 |
PROCESS OF OBTAINING QUICK-RESISTANT BORON-FREE SOLDER NICKEL BRAZING PRODUCTS FROM CORROSIVE-STEEL, SOLDER, PEAK CONNECTION AND METHOD OF ITS OBTAINING | 2015 |
|
RU2625924C2 |
METHOD OF SOLDERED CONNECTION OF ALUMINA CERAMIC WITH TITANIUM ALLOY BT1-0 | 2019 |
|
RU2717446C1 |
HETEROGENEOUS ACTIVE SOLDER FOR SOLDERING OF METAL-CERAMIC AND CERAMIC VACUUM-DENSE COMPOUNDS | 2019 |
|
RU2717766C1 |
ZIRCONIUM BASE ALLOY FOR SOLDERING | 2003 |
|
RU2252848C1 |
SOLDER FOR SOLDERING TITANIUM AND ITS ALLOYS | 0 |
|
SU1580722A1 |
SPACING GRID MAKING METHOD | 2003 |
|
RU2252846C1 |
TITANIUM-BASED SOLDER FOR SOLDERING ALLOY BASED ON NIOBIUM INTERMETALLIDE | 2015 |
|
RU2600785C1 |
ZIRCONIUM-BASE ALLOY | 1992 |
|
RU2009241C1 |
Authors
Dates
2014-05-27—Published
2013-05-17—Filed