FIELD: machine building.
SUBSTANCE: article is processed by pulse laser with efficient pulse energy of 60-500 J, pulse power density of 1.2·1010-4.3·1011 W/m2, wavelength of 1.064·10-6 m, pulse duration of 0.8·10-3 s, beam diameter of 1.2·10-3-2.5·10-3 m and distance fro irradiated point to surface being hardened of 12-30 mm.
EFFECT: higher physical-mechanical properties.
7 dwg
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF INCREASING PHYSICAL AND MECHANICAL PROPERTIES OF TOOL MATERIALS BY VOLUME PULSE LASER HARDENING | 2019 | 
 | RU2726233C1 | 
| METHOD OF HARDENING CUTTING TOOL FROM CARBIDE-CONTAINING ALLOYS BY CONTINUOUS LASER ACTION | 2018 | 
 | RU2688104C1 | 
| OPERABILITY IMPROVEMENT METHOD OF HARD-ALLOY CUTTING TOOL USING PULSE LASER TREATMENT METHOD | 2011 | 
 | RU2460811C1 | 
| METHOD FOR LASER SURFACE HARDENING OF SHAFTS WITH DIAMETER FROM 5 TO 15 mm, MADE FROM CHROMIUM-NICKEL STEELS OF AUSTENITIC-FERRITE CLASS | 2024 | 
 | RU2836274C1 | 
| METHOD OF LASER PROCESSING OF PARTS OF ROTATION BODIES FROM TOOL STEELS | 2020 | 
 | RU2734826C1 | 
| HEAT TREATMENT METHOD | 0 | 
 | SU1752784A1 | 
| METHOD FOR LASER IMPACT PROCESSING OF METAL WORKPIECE | 2024 | 
 | RU2838925C1 | 
| METHOD OF IMPROVING SURFACE CLEANLINESS OF TREATED METAL ARTICLES | 2019 | 
 | RU2740584C1 | 
| METHOD FOR LASER ALLOYING OF TOOL STEEL WITH BORON CARBIDE AND ALUMINUM POWDERS | 2022 | 
 | RU2786263C1 | 
| STEEL PIECES HARDENING METHOD | 1992 | 
 | RU2048606C1 | 
Authors
Dates
2014-05-27—Published
2013-01-09—Filed