FIELD: metallurgy.
SUBSTANCE: proposed method comprises locating of concentrate into converter and its oxidative smelting. First, matte is poured into converter to blow it with coal-air mix at coal consumption of 500 kg per ton of matte at coal-to-air ratio of 0.35 kg/m3. Concentrate is loaded on fused matte surface to blow it with air enriched with oxygen to 25 vol. % to complete smelting of concentrate. Quartz and lime flux are loaded to proceed with blowing to produce the slag and matter rich in copper, both are, now, discharged by 70% to resume melt blowing with coal-air mix.
EFFECT: simplified process.
2 tbl, 7 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING ZINC-CONTAINING COPPER MATERIALS | 2008 |
|
RU2364640C1 |
METHOD OF PROCESSING FINE-GRAIN LEAD AND LEAD-ZINC COPPER-CONTAINING SULFIDE CONCENTRATES | 0 |
|
SU1544829A1 |
HORIZONTAL CONVERTER AND COMBINED MELTING-CONVERTING METHOD | 2019 |
|
RU2734613C2 |
0 |
|
SU112514A1 | |
AUTOGENOUS CALCINATING-MELTING INSTALLATION | 2003 |
|
RU2241931C2 |
REPROCESSING CLINKER FROM ZINC PRODUCTION | 2004 |
|
RU2278174C2 |
METHOD OF AUTOGENOUS SMELTING OF SULFIDE COPPER CONCENTRATES | 2002 |
|
RU2225455C2 |
METHOD OF INTRAFURNACE STRIPPING OF SLAGS IN VANUYKOFF'S FURNACE | 1992 |
|
RU2061771C1 |
METHOD FOR COMPLEX REPROCESSING OF METAL IRON CONCENTRATE, CONTAINING NONFERROUS AND PRECIOUS METALS | 2007 |
|
RU2354710C2 |
METHOD OF PROCESSING SULFIDE CONCENTRATES | 2001 |
|
RU2199598C1 |
Authors
Dates
2014-06-20—Published
2012-12-06—Filed