FIELD: process engineering.
SUBSTANCE: invention can be used for welding or surfacing of parts from difficult-to-weld metals and alloys. Weld sections are sequentially made by step-by-step reciprocation of electrode or welding head. Length of the weld first section makes 40-60% of welding step. Electrode or welding head is turned to weld first section welding start to weld second section in length equal to said step. Note here that said first part is made at rerun over weld previous section while second section is made at article surface to produce a transition part. Then, electrode or welding head is returned for spacing equal to the weld previous section second part length. Next section is produced in length equal to welding step by rerun over second part of weld previous section and over article surface. Welding or surfacing is reiterated required number of times unless weld of preset length is produced. Last section of the weld of residual length is made by rerun over previous section second part.
EFFECT: decreased area of thermal effects, higher welding efficiency.
5 dwg, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF WELDING OF BASE STRUCTURES MANUFACTURED OF ALUMINIUM ALLOYS | 1996 |
|
RU2089364C1 |
THREE-PHASE ARC WELDING METHOD | 0 |
|
SU1798077A1 |
METHOD OF ARC WELDING | 0 |
|
SU1818180A1 |
WELDING WIRE COMPOSITION | 2010 |
|
RU2446929C1 |
METHOD OF CLADDING AND FUSION WELDING OF SUPERALLOYS | 2012 |
|
RU2610198C2 |
PROCESS FOR FUSION WELDING | 0 |
|
SU1109274A1 |
METHOD OF ELECTRIC-ARC WELDING | 1997 |
|
RU2110378C1 |
ARC WELDING METHOD | 0 |
|
SU1386400A1 |
METHOD FOR LOW-TEMPERATURE WELDING OF CAST-IRON | 1996 |
|
RU2098248C1 |
METHOD OF WELDING OF DEFECTS IN ALUMINIUM ALLOY CASTINGS | 1997 |
|
RU2109611C1 |
Authors
Dates
2014-07-10—Published
2012-07-24—Filed