FIELD: metallurgy.
SUBSTANCE: invention relates to metallurgy, particularly, to aluminium-copper alloys containing vanadium. Proposed composition contains the following substances, in wt %: Cu 3.3-4.1, Mg 0.7-1.3, V 0.01-0.16, Mn 0.01-0.7, 0.01-0.25 of at least one element defining the grainy structure and selected from the group consisting of Zr, Sc, Cr and Hf, Zn up to 1.0, Ag up to 0.6, Fe up to 0.25 and Si up to 0.25, aluminium, other elements and impurities making the rest.
EFFECT: higher strength, resistance to corrosion and fatigue crack growth.
23 cl, 11 dwg, 11 tbl, 4 ex
Title | Year | Author | Number |
---|---|---|---|
Al-Zn-Cu-Mg ALLOYS ON BASE OF ALUMINIUM, PROCEDURES FOR THEIR PRODUCTION AND IMPLEMENTATION | 2006 |
|
RU2425902C2 |
ALUMINIUM-COPPER-MAGNESIUM ALLOYS, ALLOWING SUBSIDIARY ADDITIVES OF LITHIUM | 2004 |
|
RU2359055C2 |
ALUMINIUM-LITHIUM ALLOYS OF 2XXX SERIES | 2012 |
|
RU2587009C2 |
ALLOY Al-Zn-Mg-Cu | 2004 |
|
RU2353693C2 |
IMPROVED THICK WROUGHT ALUMINIUM 7XXX ALLOYS AND METHODS FOR PRODUCTION THEREOF | 2016 |
|
RU2752487C2 |
ALLOYS OF SET 2000 WITH IMPROVED PROPERTIES OF RESISTANCE AGAINST DAMAGES FOR AEROSPACE APPLICATION | 2005 |
|
RU2379366C2 |
2XXX SERIES ALUMINUM LITHIUM ALLOYS | 2013 |
|
RU2659529C2 |
IMPROVED DENSE FORGED ALLOYS BASED ON 7XXX ALUMINUM AND METHODS FOR THEIR PRODUCTION | 2018 |
|
RU2745433C1 |
MANUFACTURING METHODS OF PRODUCTS FROM ALUMINIUM ALLOYS OF AA2000 SERIES | 2007 |
|
RU2443798C2 |
PRODUCTS FROM ALUMINIUM ALLOY, WHICH HAVE IMPROVED COMBINATIONS OF PROPERTIES | 2008 |
|
RU2465360C2 |
Authors
Dates
2014-07-27—Published
2010-01-22—Filed