FIELD: construction.
SUBSTANCE: slag includes acid electrolyte with solution density ρ=1.310 g/cm3, and slag of steel-smelting production is electric steel-smelting slag. The cement-free binder including slag of steel-smelting production, burnt rocks of mine dump and slag produced as a result of neutralisation of spent electrolytes of acid accumulators by lime, contains electric steel-smelting slag as slag of steel-smelting production, and slag contains electrolyte with solution density ρ=1.310 g/cm3 at the following ratio, wt %: burnt rocks 14, steel-smelting slag - electric steel-smelting 78, slag 8.
EFFECT: increased strength.
3 tbl
Title | Year | Author | Number |
---|---|---|---|
GROUTING MORTAR | 2017 |
|
RU2642736C1 |
STOWAGE MIXTURE COMPOSITION | 2007 |
|
RU2348814C1 |
METHOD FOR PREPARING CEMENTLESS BACKFILL MIXTURE | 2022 |
|
RU2792863C1 |
CONCRETE MIXTURE | 2008 |
|
RU2377215C1 |
STOWING MIXTURE COMPOSITION | 2018 |
|
RU2721566C1 |
METHOD OF RECYCLING FLUORO-ANHYDRITE | 2010 |
|
RU2440940C2 |
COMPOSITION OF STOWING MIXTURE | 2011 |
|
RU2455494C1 |
FAST-HARDENING CONSTRUCTION COMPOUND BASED ON STEEL SLAG | 2017 |
|
RU2647010C1 |
CLINKERLESS CEMENT | 2010 |
|
RU2430043C1 |
BINDER | 2007 |
|
RU2372302C2 |
Authors
Dates
2015-02-20—Published
2014-02-19—Filed