FIELD: metallurgy.
SUBSTANCE: weld joint is heated by sending an electric current via a weld joint up to 10 kA as current leads are fixed at different sides relative to the weld seam on the process lap of a blade and a blisk. In the process of thermal treatment they measure the temperature of the weld joint surface and adjust it by the variation of the current value within 540-620°C. The maximum permissible heating temperature is set with the condition of saving the fine-grained structure of the weld joint. The minimum permissible temperature is set with the condition of removal of residual welding stresses in a weld joint. Thermal treatment is carried out with AC current with thyristor regulation of its value.
EFFECT: invention makes it possible to increase the efficiency of removal of residual stresses of joints due to the reduced distortion of the blisk profile, and also to increase the efficiency of thermal treatment due to direct heating of the entire cross section of the weld joint by electric current of a high value.
3 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
ARGON-ARC PROCESSING OF WELDS PRODUCED BY LINEAR FRICTION WELDING | 2012 |
|
RU2524037C1 |
METHOD OF TURBO MACHINE INTEGRAL WHEEL | 2013 |
|
RU2513491C1 |
METHOD OF LINEAR FRICTION WELDING | 2014 |
|
RU2574566C1 |
METHOD OF FRICTION SEAM WELDING OF PARTS FROM TITANIUM ALLOYS | 2010 |
|
RU2456141C2 |
METHOD OF SEAM FRICTION WELDING OF BILLETS FROM TITANIUM ALLOWS FOR TURBOMACHINE MONOBLOCKS | 2010 |
|
RU2456143C2 |
METHOD OF OBTAINING BLANK OF GAS TURBINE ENGINE BLADE FOR LINEAR WELDING BY FRICTION | 2016 |
|
RU2631231C1 |
METHOD OF LINEAR FRICTION WELDING OF VANES WITH DISC TO MAKE BLISK | 2012 |
|
RU2496989C1 |
METHOD OF FRICTION SEAM WELDING OF PARTS FROM TITANIUM ALLOYS | 2010 |
|
RU2456142C2 |
DEVICE FOR SEAM WELDING BY FRICTION OF BLISKS | 2014 |
|
RU2563615C1 |
METHOD FOR MAKING ROTOR OF GAS TURBINE ENGINE | 2001 |
|
RU2196672C1 |
Authors
Dates
2015-05-20—Published
2013-11-21—Filed