FIELD: metallurgy.
SUBSTANCE: heat resistant alloy on Ni base contains in wt %: C ≤ 0.15, Si ≤ 2, Mn ≤ 3%, P ≤ 0.03, S ≤ 0.01, Cr 15 and over or below 28, Mo from 3 to 15, Co over 5 and 25 max., Al from 0.2 to 2, Ti from 0.2 to 3, Nd from f1 to 0.08 and O ≤ 0.4Nd. At that lower limit of Nd is determined by the following expression f1 = 1.7×10-5d+0.05{(Al/26.98)+(Ti/47.88)}, where d is mean grain size, mcm, and each element symbol means content in wt %.
EFFECT: alloy is characterised by increased plasticity after long-term operation at high temperatures, at that SR-cracking can be excluded.
3 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
AUSTENITIC STAINLESS STEEL | 2011 |
|
RU2507294C2 |
HEAT RESISTING IRON-CHROME-ALUMINIUM ALLOY WITH LOW SPEED OF CHROME EVAPORATION AND INCREASED HEAT RESISTANCE | 2012 |
|
RU2567144C2 |
METAL RESISTANT TO CARBURISING | 2012 |
|
RU2553136C1 |
MATERIAL OF Ni-Cr ALLOY AND SEAMLESS PETROLEUM PIPE PRODUCTS MANUFACTURED FROM IT | 2014 |
|
RU2630131C1 |
CHROME NICKEL ALUMINIUM ALLOY WITH GOOD MACHINABILITY, CREEP LIMIT PROPERTIES AND CORROSION RESISTANCE PARAMETERS | 2013 |
|
RU2599324C2 |
FOIL FROM FERRITE STAINLESS STEEL | 2013 |
|
RU2578308C1 |
FABRICABLE, HIGH STRENGTH, OXIDATION RESISTANT Ni-Cr-Co-Mo-Al ALLOYS | 2014 |
|
RU2650659C2 |
WELDED JOINT | 2015 |
|
RU2659523C2 |
WEAR-RESISTANT ALLOY FOR HIGH-TEMPERATURE APPLICATIONS | 2009 |
|
RU2479658C2 |
NICKEL CHROME ALLOY WITH GOOD MACHINABILITY, CREEP LIMIT PROPERTIES AND CORROSION RESISTANCE | 2013 |
|
RU2605022C1 |
Authors
Dates
2015-07-10—Published
2012-07-31—Filed