FIELD: chemistry.
SUBSTANCE: method of obtaining iron-chrome-phosphate product includes dissolution of 60-80 g of cast iron chips and 160-210 g of iron oxide in 650-850 g of orthophosphoric acid of 85%-90% concentration, with carrying out heating to 90°C-100°C in case of reaction slowing down, after dissolution of cast iron chips and iron oxide obtained solution is cooled, 85-115 g of chrome oxide are added, and then obtained paste of iron-chrome-phosphate product is dried and milled. Fireproof composition contains mixture of obtained iron-chrome-phosphate product, mineral filling agent and water.
EFFECT: invention makes it possible to obtain iron-chrome-phosphate product, resistant to high temperatures, which adds properties of high adhesiveness, chemical resistant and fire resistance to fireproof compositions.
2 cl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING COMPOUND METAL-PHOSPHATE PRODUCT (VERSIONS) | 2014 |
|
RU2579378C2 |
COLD-HARDENING MOULDING SAND FOR MANUFACTURING CASTING MOULDS AND CORES | 0 |
|
SU1168313A1 |
PHOSPHATE BINDER FOR PREPARING REFRACTORY COMPOSITIONS | 1997 |
|
RU2139836C1 |
SELF-HARDENABLE MIXTURE FOR PRODUCING CASTING MOULDS AND CORES | 0 |
|
SU850254A1 |
REFRACTORY MASS | 2001 |
|
RU2212387C2 |
METHOD OF REUSING ACIDIC IRON-CONTAINING SOLUTIONS | 1996 |
|
RU2110488C1 |
METHOD FOR PROCESSING OF EXHAUSTED SOLUTIONS COMPRISING COMPOUNDS OF HEXAVALENT CHROMIUM | 1996 |
|
RU2110486C1 |
COMPOSITION FOR FRICTION ASBESTOS-FREE MATERIAL | 1999 |
|
RU2147024C1 |
COLD-HARDENING MIXTURE TO PRODUCE FOUNDRY MOULDS AND RODS | 1991 |
|
RU2022678C1 |
ACID-BASE BINDING MATERIAL CONTAINING PHOSPHATE-BASED CEMENTS | 2015 |
|
RU2707316C2 |
Authors
Dates
2015-12-10—Published
2014-04-09—Filed