FIELD: woodworking industry.
SUBSTANCE: timber, which is a waste of cleaning cutting or target timber, is cut using woodworking equipment to end or longitudinal workpieces. Using the mill the outer contour of the workpieces is imparted with a shape. Subsequently, the workpieces are fed to the impregnation bath with a solution of 30-50% concentration in acetone of low molecular weight polymer in the form of epoxy resin having a molecular weight of 600-1500 and containing the hardener as 10 wt % of hexamethylenediamine per 100 wt % of resin. After impregnation for 0.5-1.5 hours the workpieces are dried in a heat chamber at a temperature of 100-120°C for 1-3 hours until complete removal of volatile components.
EFFECT: increased physical and mechanical properties of the workpieces.
1 tbl, 6 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURE OF WOODEN BLOCKS FOR PARQUET FLOORING | 2006 |
|
RU2327559C1 |
PARQUET BLANK MANUFACTURE METHOD | 1997 |
|
RU2118928C1 |
METHOD OF MANUFACTURING END FACE MEMBER FOR FINISHING FLOORS AND WALLS | 1994 |
|
RU2096171C1 |
METHOD OF PROTECTING MODIFIED-WOOD FINISHING TILES | 1999 |
|
RU2146610C1 |
METHOD FOR PRODUCTION OF PARQUET PANELS | 1994 |
|
RU2081978C1 |
METHOD FOR PRODUCING EDGED STRIPS FOR PARQUET SHIELDS OR WALL PANELS | 1994 |
|
RU2104150C1 |
METHOD TO PRODUCE END FACE BOARD PANEL ELEMENTS FROM WOOD | 2012 |
|
RU2522727C1 |
METHOD OF MAKING END BOARD ELEMENTS FROM WOOD | 2012 |
|
RU2512359C2 |
METHOD FOR MANUFACTURE OF PARQUET | 2001 |
|
RU2203801C2 |
METHOD FOR PRODUCTION OF PARQUET SHIELDS | 1994 |
|
RU2074935C1 |
Authors
Dates
2016-01-10—Published
2014-01-30—Filed