FIELD: construction.
SUBSTANCE: invention relates to compositions of mixtures for making ceramic bricks. Ceramic mixture contains the following components, wt%: beidellite fusible clay 50-70; ash-slag material 15-25; wastes of gold ore deposit 15-25. Wastes of gold ore deposit have following composition, wt%: SiO2 - 62.63; Al2O3 - 17.18; Fe2O3 - 7.84; CaO - 1.2; MgO-1.15; R2O - 6.6; ignition loss - 3.4.
EFFECT: technical result is increasing in frost resistance of brick.
1 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
CERAMIC PASTE FOR CERAMIC BRICK MANUFACTURING | 2007 |
|
RU2354627C2 |
CERAMIC MASS TO MANUFACTURE CERAMIC BRICK | 2010 |
|
RU2440317C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICK | 2014 |
|
RU2550166C1 |
CERAMIC PASTE FOR CERAMIC BRICK MANUFACTURING | 2007 |
|
RU2354626C2 |
CERAMIC MASS FOR MAKING CERAMIC BRICK | 2014 |
|
RU2555974C1 |
CERAMIC MASS FOR THE MANUFACTURE OF CERAMIC EARTHQUAKE-RESISTANT BRICKS | 2021 |
|
RU2778916C1 |
CERAMIC MASS FOR MANUFACTURE OF EARTHQUAKE-RESISTANT CERAMIC BRICKS | 2020 |
|
RU2764006C1 |
CERAMIC COMPOSITION FOR MAKING BRICK | 2015 |
|
RU2588988C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2009 |
|
RU2398752C1 |
CERAMIC PASTE FOR CERAMIC BRICK MANUFACTURING | 2007 |
|
RU2346908C2 |
Authors
Dates
2016-04-27—Published
2015-03-11—Filed