FIELD: machine building.
SUBSTANCE: method for induction hardening of tillage working element is designed for use in agricultural, construction and other industries. Hard surface tillage working element part is applied charge containing, wt%: sormite grit 40-70, iron borides 30-60, with layer thickness from 0.5 to 5.0 mm. Thereafter, article is heated in inductor by HF currents at specific power of 0.8-5.0 kW per 1 cm2 of surface with frequency equal to 1-80 kHz for 0.5-5 minutes before melting surface of charge. After heating of fusion bonded product is cooled in water.
EFFECT: higher wear resistance of tillage tool.
1 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF INDUCTIVE HARDENING AND RECONDITIONING OF PARTS | 2012 |
|
RU2507027C1 |
METHOD FOR DIFFUSION HARDENING OF STEEL PARTS | 2014 |
|
RU2589954C1 |
CHARGE FOR INDUCTION SURFACING OF WEAR-RESISTANT ALLOY | 2020 |
|
RU2755913C1 |
METHOD OF SURFACE HARDENING OF STEEL PART CONTAINING DEAD-END CAVITIES | 2014 |
|
RU2569872C1 |
METHOD OF REINFORCING STEEL COMPONENTS | 2014 |
|
RU2556805C1 |
SURFACING COMPOSITION | 2020 |
|
RU2752057C1 |
METHOD FOR LASER ALLOYING OF TOOL STEEL WITH BORON CARBIDE AND ALUMINUM POWDERS | 2022 |
|
RU2786263C1 |
METHOD FOR PRODUCING DURABLE COMPOSITE COATING ON METAL PARTS | 2020 |
|
RU2752403C1 |
METHOD OF STRENGTHENING BLADE SURFACE OF PART | 2016 |
|
RU2640515C1 |
METHOD OF INDUCTION SURFACE WELDING | 1994 |
|
RU2090326C1 |
Authors
Dates
2016-04-27—Published
2014-12-02—Filed