FIELD: mechanical engineering.
SUBSTANCE: invention relates to the field of hardening of parts by induction surfacing with wear-resistant materials. As a metal alloy, the charge contains a wear-resistant alloy of the Fe-Si-C-Cr-Cu-Mn-Ni system, obtained from acid-resistant cast iron ferrosilite grade FS-17 and high-chromium, wear-resistant cast iron grade Sormayt No. 1 and copper grade M1 with the following component ratio, wt. %: ferrosilite FS-17 55-65, Sormayt No. 1 25-20, copper M1 20-15, flux based on boron-containing components being the rest. As a flux based on boron-containing components, it contains a mixture of fused flux for induction surfacing of grade P-0.66 and boron carbide, with the following component ratio, wt. %: flux P-0.66 80-85, boron carbide 20-15.
EFFECT: increase in the wear resistance of the deposited metal under conditions of abrasive wear with alternating shock loads, a decrease in the content of scarce alloying elements (Cr, Mn) in the material, a decrease in labor intensity and an increase in manufacturability when applying a strengthening coating by induction surfacing.
2 cl, 4 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR SURFACING IRON ALUMINIDE ON STEEL SURFACE | 2018 |
|
RU2693988C1 |
METHOD OF INDUCTION BUILD-UP OF HIGH ALLOYED CHROMOUS CAST IRONS | 2014 |
|
RU2568036C2 |
POWDER THERMO-REACTIVE CHARGE FOR INDUCTION WELDING OF SOLID ALLOY | 2015 |
|
RU2637736C2 |
MIXTURE FOR INDUCTION WELDING DEPOSITION OF WEAR-RESISTANT MATERIAL | 1997 |
|
RU2123920C1 |
METHOD OF SURFACE HARDENING OF STEEL PART CONTAINING DEAD-END CAVITIES | 2014 |
|
RU2569872C1 |
ELECTRODE FOR WEAR-RESISTANT ELECTRIC ARC SURFACING | 2021 |
|
RU2769682C1 |
METHOD OF PRODUCING MOULDED STEEL PART | 2015 |
|
RU2622503C2 |
MIXTURE FOR INDUCTION WELDING | 2014 |
|
RU2581698C1 |
METHOD FOR CASTING | 2016 |
|
RU2632500C2 |
METHOD FOR ALLOYING THIN-WALLED IRON CASTINGS | 2022 |
|
RU2784305C1 |
Authors
Dates
2021-09-22—Published
2020-12-25—Filed