FIELD: metallurgy.
SUBSTANCE: invention relates to magnesium-thermal production of spongy titanium. Method comprises pouring magnesium into a retort, supply of titanium tetrachloride and conducting the process of recovery of titanium tetrachloride by magnesium at supply of titanium tetrachloride in an amount less than its theoretical amount 1.0-1.25 times. After finishing the supply of titanium tetrachloride the magnesium chloride is drained, maintained for 1-1.5 hours and magnesium chloride is additionally drained. Block of spongy titanium is subjected to vacuum-thermal purification from impurities. Then the block is removed from the retort, the middle part is crushed and screened into fraction to produce fractions sized -25+12 mm and -12+2 mm with chlorine content of not more than 0.02 wt%. If necessary, the obtained fractions of -25+12 mm and -12+2 mm are mixed into a common fraction batch sized -25+2 mm.
EFFECT: provided is reduced content of impurities of chlorine and its compounds in spongy titanium 4 times.
1 cl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
SPONGY TITANIUM OBTAINING METHOD | 2011 |
|
RU2466198C1 |
ALLOY SPONGY TITANIUM OBTAINING METHOD | 2016 |
|
RU2635211C1 |
METHOD FOR PRODUCTION OF SPONGY TITANIUM | 2014 |
|
RU2586187C1 |
METHOD OF PRODUCING TITANIUM BRIQUETTES WITH FLUX | 2019 |
|
RU2695397C1 |
METHOD OF VACUUM SEPARATION OF SPONGY TITANIUM AND DEVICE FOR REALIZATION OF THIS METHOD | 2004 |
|
RU2273674C1 |
PROCESSING METHOD OF TITANIC JAW | 2007 |
|
RU2353686C1 |
METHOD OF PRODUCING LOWER TITANIUM CHLORIDES IN MIXTURE OF MOLTEN METAL CHLORIDES AND DEVICE TO THIS END | 2007 |
|
RU2370445C2 |
TITANIUM SPONGE MAGNESIUM-REDUCED PRODUCTION APPARATUS | 2005 |
|
RU2288962C1 |
METHOD FOR PRODUCTION OF SPONGE TITANIUM ALLOYED WITH OXYGEN | 1996 |
|
RU2106418C1 |
METHOD OF PRODUCING TITANIUM SPONGE AND DEVICE TO THIS END | 2013 |
|
RU2534482C2 |
Authors
Dates
2016-10-10—Published
2015-06-22—Filed