FIELD: metallurgy.
SUBSTANCE: present invention describes a method for two-step sodium calcining of vanadium-containing material, including successive execution of a first calcining step and a second step of calcining raw material. Raw material is a mixture of vanadium-containing material with addition of sodium salt. Temperature at second calcining step is 760–800 °C, wherein temperature at second calcining step is higher than that at first calcining step, and duration of both first calcining step, and second calcining step is 60–300 minutes.
EFFECT: technical result is improved process of converting vanadium due to elimination of agglomeration and sticking of material when calcining.
9 cl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MIXING AND SODIUM-CALCINING VANADIUM-CONTAINING MATERIAL | 2015 |
|
RU2608248C2 |
METHOD FOR TWO-STEP CALCINATION OF VANADIUM-CONTAINING MATERIAL | 2015 |
|
RU2607292C2 |
METHOD OF CALCINING VANADIUM-CONTAINING MATERIAL | 2015 |
|
RU2607290C2 |
METHOD OF PRODUCING VANADIUM OXIDE | 2009 |
|
RU2454369C1 |
METHOD OF PRODUCING VANADIUM OXIDE THROUGH EXTRACTION | 2009 |
|
RU2456241C2 |
METHOD OF PRODUCING VANADIUM OXIDE USING ION EXCHANGE TO RECYCLE WASTE WATER | 2009 |
|
RU2454368C1 |
METHOD OF EXTRACTION OF VANADIUM FROM VANADIUM-CONTAINING CARBONIZED LEACHING SOLUTION AND REUSE OF RESIDUAL VANADIUM PRECIPITATION LIQUID | 2022 |
|
RU2807981C1 |
METHOD OF PREPARING VANADIUM OXIDE | 2014 |
|
RU2562989C1 |
METHOD OF FABRICATING VANADIUM PRODUCTS BY FLUIDISATION | 2008 |
|
RU2441083C1 |
METHOD OF EXTRACTING VANADIUM FROM VANADIUM SLAG WITH HIGH CONTENT OF CALCIUM AND PHOSPHORUS | 2019 |
|
RU2743355C1 |
Authors
Dates
2017-01-10—Published
2015-05-21—Filed