FIELD: metallurgy.
SUBSTANCE: forgings manufacturing method from titanium alloys includes extrusion of billet under isothermal conditions at the same temperature of heating the billet and die and subsequent isothermal forging of the extruded billet. The extrusion and isothermal forging is performed at the heating temperature of the die and billet 800-830 °C±40 °C at average strain rate not more than 0.3 mm/s.
EFFECT: reduce of alloy deformation resistance and increase of dimensional stability of dies, manufacturing of blade forgings with a fine-grained structure.
1 dwg,1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MANUFACTURING BLADES FROM TWO-PHASE TITANIUM ALLOYS | 2021 |
|
RU2759280C1 |
METHOD FOR MANUFACTURING BLADES FROM A TWO-PHASE TITANIUM ALLOY | 2020 |
|
RU2760328C1 |
FORDING OF BLADES FROM TWO-PHASE TITANIUM ALLOY | 2013 |
|
RU2525961C1 |
METHOD OF TREATMENT OF CAST HYPEREUTECTOID ALLOYS ON BASE OF TITANIUM ALUMINIDES γ-TiAl AND αTlAl | 2001 |
|
RU2203976C2 |
METHOD OF PRODUCT RECEIVING FROM α+β-TITANIUM ALLOY | 2008 |
|
RU2368700C1 |
METHOD OF MAKING BLOWER COMPOSITE BLADE LEADING EDGE STRAP | 2012 |
|
RU2503519C1 |
METHOD OF FORGING WORKPIECES WITH ULTRA-FINE-GRAINED STRUCTURE OF TWO-PHASE TITANIUM ALLOYS | 2019 |
|
RU2707006C1 |
METHOD OF PUNCHING OF BLANKS FROM NANOSTRUCTURED TITANIUM ALLOYS | 2008 |
|
RU2382686C2 |
METHOD OF MAKING STAMPING OF GAS TURBINE ENGINE BLADE FROM TWO-PHASE TITANIUM ALLOY | 2023 |
|
RU2818513C1 |
DIE FOR HOT-MOLDING OF PARTS FROM TITANIUM ALLOYS | 2010 |
|
RU2456112C2 |
Authors
Dates
2017-03-24—Published
2016-04-04—Filed