FIELD: chemistry.
SUBSTANCE: polyurethane rubber mixture in the first version was obtained on the basis of saturated urethane rubber, 100 wt p of which includes stearic acid in an amount of 1.0 parts by weight, di-tert-butyl peroxyisopropylbenzene in an amount of 12.5 wt p and carbon black in an amount of 42.0 wt p in the second version, the polyurethane rubber mixture is obtained on the basis of saturated urethane rubber, per 100 wt p which includes stearic acid in an amount of 1.0 wt p, di-tert-butyl peroxyisopropylbenzene in an amount of 12.5 wt p, silica filler in an amount of 35.0 wt p and iron-oxide pigment in an amount of 3.0 wt p.
EFFECT: reducing the explosion hazard of the production process.
3 cl, 2 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
FIRE-RESISTANT RUBBER MIXTURE | 2012 |
|
RU2540597C2 |
FIRE-RESISTANT RUBBER MIXTURE | 2011 |
|
RU2472821C1 |
RUBBER MIXTURE BASED ON HIGH MOLECULAR METHYL VINYL SILOXANE RUBBER | 2011 |
|
RU2468048C1 |
CURABLE RUBBER COMPOUND BASED ON CARBON-CHAIN POLYMER FOR MANUFACTURING COLORED GRANULATE | 2004 |
|
RU2270210C1 |
COMPOSITION FOR FORMING OF THE POLYURETHANE COATINGS SURFACE LAYER | 2017 |
|
RU2649645C2 |
THERMOPLASTIC RUBBER MANUFACTURING PROCESS | 2004 |
|
RU2312872C2 |
CERAMICS-FORMING RUBBER MIXTURE (VERSIONS) | 2012 |
|
RU2519379C2 |
RUBBER COMPOSITION | 2015 |
|
RU2608399C1 |
RUBBER COMPOSITION | 2017 |
|
RU2671321C1 |
0 |
|
SU359256A1 |
Authors
Dates
2017-05-17—Published
2015-12-21—Filed