FIELD: metallurgy.
SUBSTANCE: alloy contains wt %: carbon up to 0.2; manganese from more than 3.0 to 20; silicon from 0.1 to 1.0; chromium from 14.0 to 28.0; nickel from more than 15.0 to 38.0; molybdenum from more than 3.0 to 6.5; copper from 0.1 to 3.0; nitrogen from 0.08 to 0.9; tungsten from 0.1 to 5.0; cobalt from 0.5 to 5.0; titanium up to 1.0; boron up to 0.05; phosphorus up to 0.05; sulfur up to 0.025; iron and incidental impurities are the rest.
EFFECT: alloy has high corrosion resistance and mechanical properties.
31 cl, 2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
HIGH-STRENGTH, CORROSION-RESISTANT AUSTENITIC ALLOYS | 2012 |
|
RU2731395C2 |
METHODS FOR TREATING ALLOYS | 2014 |
|
RU2690246C2 |
THERMOMECHANICAL TREATMENT OF HIGH STRENGTH NON-MAGNETIC CORROSION-RESISTANT MATERIAL | 2014 |
|
RU2745050C2 |
THERMOMECHANICAL PROCESSING OF HIGH-STRENGTH NON-MAGNETIC CORROSION-RESISTANT MATERIAL | 2014 |
|
RU2644089C2 |
AUSTENITIC STAINLESS STEEL WITH LOW CONTENT OF NICKEL AND INCLUDING STABILISING ELEMENTS | 2008 |
|
RU2461641C2 |
SPARINGLY ALLOYED AUSTENITIC STAINLESS STEEL | 2008 |
|
RU2458178C2 |
METHODS FOR PROCESSING METAL ALLOYS | 2014 |
|
RU2675877C1 |
HIGH-STRENGTH TITANIUM ALLOYS | 2019 |
|
RU2774671C2 |
AUSTENITIC STAINLESS STEEL | 2010 |
|
RU2586366C2 |
SPARINGLY ALLOYED CORROSION-RESISTANT AUSTENITIC STAINLESS STEEL | 2008 |
|
RU2450080C2 |
Authors
Dates
2017-05-30—Published
2012-11-28—Filed