FIELD: machine engineering.
SUBSTANCE: pre-hardening, tempering and coating the product with a vacuum spraying method, cryogenic treatment of the product in a nitrogen gas environment at a temperature of -153 to -196°C for more than 24 hours followed with heating in it to room temperature are carried out, then a low temper is carried out at a temperature of 150 to 180°C followed by air cooling.
EFFECT: increase of products wear resistance and increase of operational durability.
2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MAKING THIN-WALL SHELLS FROM ALLOYED STEELS | 2019 |
|
RU2710311C1 |
METHOD OF CHEMICO-THERMAL TREATMENT OF SMALLSIZED CUTTING TOOLS MANUFACTURED FROM ALLOYED STEELS | 2001 |
|
RU2203982C2 |
METHOD FOR HEAT TREATMENT OF STEEL | 0 |
|
SU1133306A1 |
METHOD OF HARDENING OBJECTS OF CARBON, ALLOYED, HIGH-ALLOY, AND QUICK- CUTTING STEELS, AND HARD ALLOYS | 1996 |
|
RU2100456C1 |
METHOD OF THERMO-MAGNETIC TREATMENT OF ARTICLES MADE FROM HIGH-SPEED TOOL STEEL | 2004 |
|
RU2273670C1 |
TOOL STEELS THERMAL PROCESSING METHOD | 1991 |
|
RU2017838C1 |
METHOD OF TREATING CUTTING TOOL | 0 |
|
SU1323590A1 |
METHOD OF HEAT TREATMENT OF HIGH-SPEED STEELS | 0 |
|
SU1788980A3 |
METHOD OF MAKING AXIALLY SYMMETRIC THIN-WALL SHELLS AND DEVICE FOR MAKING AXIALLY SYMMETRIC THIN-WALL SHELLS | 2019 |
|
RU2727370C1 |
METHOD FOR PRODUCTION AND RECOVERY OF DEFORMING TOOL FOR ROTARY DRAWING | 2016 |
|
RU2635988C1 |
Authors
Dates
2017-06-29—Published
2016-10-18—Filed