FIELD: metallurgy.
SUBSTANCE: method involves heat treatment of the steel powder at a temperature of 900-1200°C in a hydrogen medium and cooling in an argon medium. Prior to heat treatment of steel powder at a temperature of 900-1200°C the steel powder is heated up to a temperature of 600-750°C in argon medium and held in carbon tetrachloride medium at a temperature of 600-750°C for 10-30 minutes. The heat treatment of the steel powder is carried out at a temperature of 900-1200°C in hydrogen medium for 40-60 minutes.
EFFECT: reduction of labour intensity and duration of the powder production process.
4 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING TITANIUM POWDER | 2015 |
|
RU2628228C2 |
METHOD OF MOLYBDENUM POWDER PRODUCTION | 2007 |
|
RU2358030C2 |
METHOD OF PRODUCING METAL POWDER WITH REDUCED OXYGEN CONTENT | 2005 |
|
RU2414327C2 |
METHOD FOR THERMOCHEMICAL TREATMENT OF METAL POWDERS FOR PRODUCING STEELS AND HEAT-RESISTANT ALLOYS HARDENED WITH DISPERSED OXIDES | 2019 |
|
RU2780653C2 |
METHOD OF PRODUCING CATALYST FOR REGENERATION OF NITROGEN OXIDE | 0 |
|
SU886965A1 |
METHOD FOR PREPARING METAL NEODYMIUM FROM ITS OXIDE | 2016 |
|
RU2634820C2 |
METHOD OF MANUFACTURING COMPOSITE MATERIAL WITH METAL MATRIX ON THE BASE OF ALUMINIUM | 0 |
|
SU1838441A3 |
METHOD FOR COATING OF SUPERABRASIVE WITH METAL | 2001 |
|
RU2247794C2 |
METHOD FOR ALUMINUM COATING IRON POWDER | 2017 |
|
RU2675711C1 |
RETARDED METAL POWDERS OR POWDER-LIKE ALLOYS, METHOD OF THEIR PRODUCTION AND REACTOR POT | 2009 |
|
RU2492966C2 |
Authors
Dates
2017-07-11—Published
2015-12-10—Filed