SUBSTANCE: method for purifying aluminium-containing chloride solutions from iron involves, at least, one stage of electrochemical purification of aluminium chloride solutions. Electrochemical purification is carried out at pH of 1.0-3.0, the cathode current density of 0.001-0.150 A/cm2 and the anodic current density of 0.015-0.200 A/cm2. Herewith the process temperature is 20-97°C.
EFFECT: invention allows to increase the purification degree of aluminium-containing chloride solutions from iron, increase the efficiency of the process and reduce consumption of electricity.
4 cl, 1 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING ALUMINUM METAL AND POLYSILICON FROM MEDIUM CONTAINING SILICON AND ALUMINUM | 2022 |
|
RU2826180C2 |
METHOD FOR PRODUCING ALUMINA, MAINLY FROM HIGH-SILICA BAUXITE | 2022 |
|
RU2801847C1 |
MANGANESE DIOXIDE PRODUCTION PROCESS | 2000 |
|
RU2172791C1 |
TECHNOLOGY OF REMOVAL OF NOBLE METALS | 2000 |
|
RU2198947C2 |
METHOD TO EXTRACT GALLIUM FROM GALLIUM-CONTAINING SLIMES | 1990 |
|
RU2037547C1 |
METHOD FOR ALUMINIUM RECYCLING BY SCRAP MELT ELECTROLYSIS AND A DEVICE FOR IMPLEMENTING THIS METHOD | 2022 |
|
RU2796566C1 |
METHOD OF PRODUCTION OF ELECTROLYTIC NICKEL | 2005 |
|
RU2303086C2 |
NICKEL CHLORIDE PRODUCTION METHOD | 2019 |
|
RU2711068C1 |
METHOD FOR PROCESSING SECONDARY GOLD-CONTAINING MATERIAL TO PURE GOLD | 2001 |
|
RU2176279C1 |
METHOD FOR PLASMA ELECTROCHEMICAL PROCESSING OF GRAPHITE FROM USED LITHIUM-ION BATTERIES | 2023 |
|
RU2825576C1 |
Authors
Dates
2017-07-14—Published
2016-06-23—Filed