FIELD: metallurgy.
SUBSTANCE: method of nitridation of products from titanic alloys in a glow discharge involves carrying out of the noted nitriding in a nitrogen-argon gas mixture, using the noted nitrogen-argon gas mixture with a percentage ratio of 60% N2 to 40% Ar, and the noted nitriding in a glow discharge is carried out in magnetic field at a temperature of 650-750°C for 4 hours, voltage in the discharge gap of 450-550 V and pressure in a vacuum chamber of 10-1-1 Pa.
EFFECT: process of surface saturation with nitrogen ions during ion nitriding of titanic alloys is intensified, and a developed diffusion zone on a titanium base of the order of 50-70 mcm is obtained.
1 dwg, 1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF ION NITRATION OF TITANIUM ALLOYS | 2015 |
|
RU2611003C1 |
METHOD FOR LOW-TEMERATURE ION NITRIDING OF TITANIUM ALLOYS WITH CONSTANT PUMPING OF A GAS MIXTURE | 2018 |
|
RU2687616C1 |
INTENSIFICATION METHOD OF LOW-TEMPERATURE ION NITRIDING OF ITEMS FROM TITANIUM ALLOYS | 2019 |
|
RU2717124C1 |
METHOD FOR LOW-TEMPERATURE ION NITRIDING OF TITANIUM ALLOYS | 2017 |
|
RU2633867C1 |
METHOD FOR HIGH DENSITY PLASMA NITRIDNG | 2015 |
|
RU2611251C2 |
PROCEDURE FOR LOW TEMPERATURE NITRIDING IN PLASMA OF NON-SELF-MAINTAINED ARC DISCHARGE OF LOW PRESSURE OF TITANIUM ALLOYS BT6 AND BT16 | 2010 |
|
RU2434074C1 |
METHOD OF ION-PLASMA NITRIDING OF ARTICLES FROM TITANIUM OR TITANIUM ALLOY | 2018 |
|
RU2686975C1 |
PROCEDURE FOR LOW TEMPERATURE NITRIDING IN PLASMA OF NON-SELF-MAINTAINED ARC DISCHARGE OF LOW PRESSURE OF TECHNICALLY PURE TITANIUM BT1-0 | 2010 |
|
RU2434075C1 |
METHOD FOR HIGH-TEMPERATURE NITRIDING OF ITEMS MADE FROM TITANIUM ALLOYS | 2015 |
|
RU2611607C2 |
MODIFICATION METHOD OF SURFACE OF ITEMS FROM TITANIUM ALLOYS IN VACUUM | 2014 |
|
RU2562185C1 |
Authors
Dates
2017-07-14—Published
2015-11-02—Filed