FIELD: chemistry.
SUBSTANCE: heat-accumulating composition includes (in wt %) lithium fluoride (9.80-10.10), lithium sulfate (66.20-67.10), sodium chloride (22.80-23.90) and has the operability in the temperature range of 447-451°C.
EFFECT: invention provides the development of the composition capable to store and release the thermal energy at 447-451 degrees, and increase of its heat-accumulating capacity.
1 tbl, 1 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
HEAT-ACCUMULATING COMPOSITION | 2017 |
|
RU2655002C1 |
HEAT-ACCUMULATING COMPOSITION | 2017 |
|
RU2675566C1 |
HEAT-ACCUMULATING COMPOSITION | 2023 |
|
RU2822273C1 |
HEAT-ACCUMULATING COMPOSITION | 2012 |
|
RU2492206C1 |
HEAT-RETAINING COMPOSITION | 2006 |
|
RU2326920C2 |
HEAT CARRIER FROM HALIDES OF ALKALI METALS | 2022 |
|
RU2817998C2 |
HEAT-ACCUMULATING MIXTURE OF LITHIUM, SODIUM AND CALCIUM HALIDES | 2023 |
|
RU2819041C1 |
HEAT-STORAGE COMPOSITION | 2004 |
|
RU2272822C1 |
HEAT-ACCUMULATING COMPOSITION | 2011 |
|
RU2458096C1 |
HEAT ACCUMULATING MATERIAL | 2018 |
|
RU2703220C1 |
Authors
Dates
2017-08-21—Published
2016-02-18—Filed