FIELD: chemistry.
SUBSTANCE: for obtaining products from high-strength ceramics, 2-5 wt % of a concentrated solution of lithium hydroxide is added to a mixture of a plasma-chemical ultradisperse powder of tetragonal zirconium oxide (75-82 wt %), alumina (15-20 wt %) and lithium oxide (3-5 wt %), the mixture is dried at a temperature of 120-200°C for 24 hours. The semifinished product is crushed and pressed into preforms in a mould at a pressure of 40-80 MPa. The billets are sintered in air at 1500-1750°C for 15-40 minutes.
EFFECT: increasing the strength of products.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
PRODUCTION METHOD OF ARTICLES FROM HIGH-TENSILE CERAMICS | 2016 |
|
RU2626866C1 |
METHOD OF MANUFACTURE OF THE STRONG CERAMICS | 2004 |
|
RU2286316C2 |
METHOD OF DOPING ALUMOOXIDE CERAMICS | 2013 |
|
RU2525889C1 |
HIGH-STRENGTH CERAMICS | 2016 |
|
RU2636336C2 |
METHOD OF MAKING SILICON NITRIDE CERAMIC WITH CALCIUM ALUMINATE SINTERING ADDITIVE WITH LOW MELTING | 2019 |
|
RU2734682C1 |
BLEND FOR PREPARING CERAMICS | 1999 |
|
RU2164503C2 |
METHOD OF MAKING ALUMINIUM NITRIDE-BASED HEAT-CONDUCTING CERAMIC | 2014 |
|
RU2587669C2 |
CERAMIC MATERIAL FOR ELECTRICAL SWITCHING DEVICES | 2022 |
|
RU2818182C2 |
METHOD OF PRODUCING ALUMINIUM NITRIDE-BASED HEAT-CONDUCTING CERAMIC | 2010 |
|
RU2433108C1 |
COMPOSITE CERAMIC MATERIAL | 2007 |
|
RU2341494C2 |
Authors
Dates
2017-11-03—Published
2016-03-17—Filed