FIELD: chemistry.
SUBSTANCE: sintered refractory product consists of an aggregate bound by a matrix, and contains oxides in percentage by weight: more than 65 of Cr2O3, less than 35 of Al2O3, 1 or more of ZrO2, at least 20 wt % of which is stabilized in the cubic and/or tetragonal form, 0.1 or more of Y2O3, acting as a stabiliser of zirconium oxide ZrO2, less than 1.9% of HfO2, wherein the total content of chromium oxide, aluminium oxide, and zirconium oxide Cr2O3+Al2O3+ZrO2 is more than 90 wt %. The product contains a coactivator that is active or inactive as a zirconium stabiliser selected from CaO, MgO,TiO2, and mixtures thereof, wherein the total content of calcium oxide, magnesium oxide, and titanium oxide CaO+MgO+TiO2 is less than 6.0 wt % and more than 0.5 wt %, and more than 50 wt % of yttrium oxide and co-activator are present in the matrix.
EFFECT: improving the stability of refractory materials for slag corrosion and temperature changes.
24 cl, 16 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
INTERNAL COATING OF REACTOR-GASIFIER | 2009 |
|
RU2537621C2 |
GASIFIER INNER SURFACE LINING | 2006 |
|
RU2403229C2 |
BAKED AND ALLOYED PRODUCED BASED ON ZIRCON + NbO OR TaO | 2007 |
|
RU2453519C2 |
DOPED SINTERED ARTICLE BASED ON ZIRCON AND ZIRCONIUM DIOXIDE | 2007 |
|
RU2456254C2 |
ZIRCONIUM DIOXIDE POWDER | 2010 |
|
RU2532818C2 |
ZIRCONIUM DIOXIDE-BASE SINTERED MATERIAL AND METHOD OF ITS MAKING | 1999 |
|
RU2201906C2 |
FIREPROOF BLOCK FOR GLASS-MELTING FURNACE | 2009 |
|
RU2527947C2 |
MELTED PARTICLES OF ALUMINIUM OXIDE AND ZIRCONIUM OXIDE | 2010 |
|
RU2543846C2 |
CERAMIC MATERIAL | 2014 |
|
RU2681020C1 |
COMPOSITE CERAMIC MATERIAL FOR HIGH-TEMPERATURE APPLICATION (VERSIONS) | 2007 |
|
RU2336245C1 |
Authors
Dates
2018-01-25—Published
2013-10-15—Filed