FIELD: chemistry.
SUBSTANCE: invention can be used in chemical industry. Lead titanate is obtained from lead nitrate and titanium dioxide. Initial reagents are homogenized for 20 minutes on a knife grinder or on a planetary mill. Solid-phase synthesis is carried out at a temperature of 450 °C for 60 minutes.
EFFECT: process does not use organic solvents, simplifies the process of preparing the initial reagents and reduces the temperature of the synthesis.
1 cl, 3 ex, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
FINELY DISPERSED LEAD-ZIRCONIUM TITANATES, ZIRCONIUM TITANATE HYDRATES AND ZIRCONIUM TITANATES AND PRODUCTION METHOD THEREOF | 2005 |
|
RU2415083C2 |
PREPARATION OF NANOSTRUCTURED MATERIALS BASED ON BaZrO | 2023 |
|
RU2808853C1 |
METHOD OF PRODUCING NANOPOWDERS OF COMPOUNDS BASED ON TITANIUM, LEAD AND ZIRCONIUM OXIDES | 2008 |
|
RU2379259C1 |
METHOD FOR OBTAINING BARIUM-CALCIUM ZIRCONATE-TITANATE POWDER FOR ADDITIVE MANUFACTURING | 2022 |
|
RU2801240C1 |
METHOD OF OBTAINING NANODISPERSE METAL OXIDES | 2012 |
|
RU2538585C2 |
METHOD OF PRODUCING SEGNETOCERAMIC MATERIALS | 0 |
|
SU829603A1 |
METHOD FOR PRODUCTION OF ZIRCON CONTAINING ISOMORPHOUS IMPURITIES | 2022 |
|
RU2776896C1 |
METHOD FOR PRODUCING LUMINESCENT MATERIAL FOR GENERATING RESULTING WHITE LIGHT IN LIGHT EMITTING DIODES | 2013 |
|
RU2553868C2 |
METHOD OF OBTAINING THE RUTILIZING GERMS | 2016 |
|
RU2622302C1 |
COMPOUND FOR PRODUCING FERROELECTRIC MATERIAL | 2007 |
|
RU2356838C2 |
Authors
Dates
2018-06-05—Published
2017-03-28—Filed