FIELD: textile and paper.
SUBSTANCE: invention relates to a method of producing paper. Method involves producing a pulp and forming a paper sheet from the pulp. At least one polymer which is functionalised with aldehyde is added before and/or after forming the sheet to the mass. Water-soluble acid is added to the formed paper sheet. Water-soluble acid has a relative acidity higher than 0.05 g/kg of dry paper.
EFFECT: higher strength of paper in wet condition.
27 cl, 6 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR INCREASING PAPER STRENGTH | 2014 |
|
RU2667287C1 |
COMPOSITIONS AND METHODS OF MAKING PAPER PRODUCTS | 2012 |
|
RU2605971C2 |
SOFTENER COMPOSITION | 2016 |
|
RU2700056C1 |
PAPER AND METHODS FOR PRODUCTION OF PAPER | 2012 |
|
RU2581862C2 |
FIBER WEB OF PAPER OR CARTON AND ITS MANUFACTURE METHOD | 2013 |
|
RU2621113C2 |
HYDROPHOBICALLY DRESSED FIBER MATERIAL AND METHOD FOR PRODUCING LAYER OF DRESSED MATERIAL | 2013 |
|
RU2635615C2 |
METHODS FOR EVALUATIG PERFORMANCES OF CREPING ADHESIVE FILM AND METHOD FOR MODIFYING CREPING ADHESIVE FILM | 2013 |
|
RU2615640C2 |
FOAM APPLICATION OF STRENGTHENING ADDITIVES ON PAPER PRODUCTS | 2018 |
|
RU2795510C2 |
METHOD FOR INCREASING DIMENSIONAL STABILITY OF A PAPER OR CARDBOARD PRODUCT | 2017 |
|
RU2746735C2 |
CELLULOSE NANOFILAMENTS WITH HIGH COEFFICIENT OF DRAWING AND PRODUCTION METHODS THEREOF | 2012 |
|
RU2596521C2 |
Authors
Dates
2019-08-01—Published
2016-02-16—Filed