FIELD: metallurgy.
SUBSTANCE: workpiece of titanium alloy fastening product includes subjected to hot rolling, treatment for solid solution and aging of alpha/beta titanium alloy consisting essentially of, wt. %: from 3.9 to 4.5 of aluminium, from 2.2 to 3.0 of vanadium, from 1.2 to 1.8 of iron, from 0.24 to 0.3 of oxygen, to 0.08 of carbon, to 0.05 nitrogen, not more than 0.3 other elements in total, titanium and random impurities, wherein other elements consist essentially of: one or more of tin, zirconium, molybdenum, chromium, nickel, silicon, copper, niobium, tantalum, manganese and cobalt, wherein the weight percentage of each such element is 0.1 or less, and boron and yttrium, wherein the weight percentage of each such element is less than 0.005. Fastener article has ultimate tensile strength of at least 180 ksi (1241 MPa) and double-shear strength of at least 108 ksi (744.6 MPa).
EFFECT: invention relates to metallurgy, namely to titanium alloys having high strength/weight ratio, which can be used for making fasteners.
12 cl, 5 dwg, 4 tbl, 7 ex
Title | Year | Author | Number |
---|---|---|---|
HIGH STRENGTH ALPHA/BETA TITANIUM ALLOY FASTENERS AND FASTENER STOCK | 2011 |
|
RU2581332C2 |
TREATMENT OF ALPHA/BETA TITANIUM ALLOYS | 2011 |
|
RU2575276C2 |
HIGH STRENGTH AND DUCTILITY ALPHA/BETA TITANIUM ALLOY | 2011 |
|
RU2616676C2 |
TITANIUM ALLOYS FOR FASTENERS | 2015 |
|
RU2618016C2 |
HIGH STRENGTH TITANIUM ALLOY WITH ALPHA-BETA STRUCTURE | 2015 |
|
RU2657892C2 |
HIGH-STRENGTH TITANIUM ALLOY WITH ALPHA-BETA STRUCTURE | 2015 |
|
RU2725395C1 |
PROCESSING OF ALPHA-BETA-TITANIUM ALLOYS | 2016 |
|
RU2725391C2 |
HOT STRAIGHTENING BY STRETCHING OF HIGH-TENSILE TITANIUM ALLOY TREATED IN FIELD OF ALPHA/BETA PHASES | 2011 |
|
RU2538467C2 |
HIGH-STRENGTH TITANIUM ALLOY FOR ADDITIVE MANUFACTURING | 2018 |
|
RU2797351C2 |
TREATMENT OF ALLOYS TITANIUM-ALUMINUM-VANADIUM AND PRODUCT MADE BY MEANS OF IT | 2004 |
|