FIELD: chemistry.
SUBSTANCE: modified wood fibre treated with acetic anhydride, suitable for the manufacture of wood products, which has a moisture content of about 5 to about 8.5 wt. %.
EFFECT: present invention does not include wood fibre where fibre from a non-acetylated source is mixed in with the acetylated wood fibre.
9 cl, 3 dwg, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS FOR MANUFACTURING PRODUCTS FROM ACETYLATED WOOD FIBRE | 2014 |
|
RU2717224C2 |
METHOD FOR CONTINUOUS ACETYLATION OF ELEMENTS FROM WOOD | 2016 |
|
RU2725674C2 |
METHOD OF WOOD ACETYLATION | 2016 |
|
RU2719997C2 |
ACETYLATION OF WOOD PARTS | 2011 |
|
RU2569536C2 |
METHOD OF PRODUCING PLATE BASED ON WOOD MATERIAL WITH REDUCED EXTRACTION OF VOLATILE ORGANIC COMPOUNDS | 2016 |
|
RU2689571C1 |
PLATE BASED ON A WOOD MATERIAL WITH REDUCED RELEASE OF VOLATILE ORGANIC COMPOUNDS (VOC) AND APPLICATION THEREOF | 2019 |
|
RU2766678C2 |
BINDER FOR PULP-CONTAINING MATERIALS | 2018 |
|
RU2803520C2 |
BINDING COMPOSITION AND USE THEREOF IN WOOD COMPOSITE BOARDS | 2016 |
|
RU2709364C2 |
METHOD FOR PRODUCTION OF MECHANICAL WOOD PULP SUITABLE FOR MANUFACTURING OF PAPER OR CARDBOARD | 2006 |
|
RU2391453C2 |
METHOD FOR WOOD ACETYLATION AND ACETYLATED WOOD | 2013 |
|
RU2621044C2 |
Authors
Dates
2020-03-16—Published
2014-02-20—Filed