FIELD: metallurgy.
SUBSTANCE: invention relates to metallurgy, namely, to creep-resistant titanium alloys. Titanium alloy contains, in mass percentages as calculated for the total mass of the alloy: from 5.5 to 6.5 aluminium, from 1.5 to 2.5 tin, from 1.3 to 2.3 molybdenum, from 0.1 to 10.0 zirconium, from 0.01 to 0.30 silicon, from 0.1 to 2.0 germanium, titanium and impurities, wherein the titanium alloy contains intermetallic precipitation containing zirconium, silicon and germanium.
EFFECT: alloy is characterised by high creep resistance under high temperatures.
27 cl, 4 dwg, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
HIGH-TEMPERATURE TITANIUM ALLOYS | 2019 |
|
RU2772375C2 |
HIGH-STRENGTH TITANIUM ALLOYS | 2019 |
|
RU2774671C2 |
HIGH-STRENGTH, CORROSION-RESISTANT AUSTENITIC ALLOYS | 2012 |
|
RU2731395C2 |
PROCESSING OF ALPHA-BETA-TITANIUM ALLOYS | 2016 |
|
RU2725391C2 |
HIGH-STRENGTH, CORROSION-RESISTANT AUSTENITIC ALLOYS | 2012 |
|
RU2620834C2 |
TITANIUM ALLOY | 2016 |
|
RU2703756C2 |
AUSTENITE STAINLESS STEEL | 2006 |
|
RU2429308C2 |
SHEET BETA-TITANIUM ALLOY TO APPLICATE INCREASING TEMPERATURE | 2016 |
|
RU2686496C1 |
METHODS FOR TREATING ALLOYS | 2014 |
|
RU2690246C2 |
THERMOMECHANICAL TREATMENT OF HIGH STRENGTH NON-MAGNETIC CORROSION-RESISTANT MATERIAL | 2014 |
|
RU2745050C2 |
Authors
Dates
2022-05-18—Published
2019-06-17—Filed