FIELD: powder metallurgy.
SUBSTANCE: production of hard alloys. The method for producing a tungsten-titanium-cobalt hard alloy includes obtaining an alloy as a result of spark plasma sintering of powders obtained by electroerosive dispersion of T5K10 alloy waste in water at a temperature T=1200°C, a pressure P=40 MPa and a holding time t=10 min.
EFFECT: providing an increase in the physical and mechanical properties of the alloy.
1 cl, 6 dwg, 3 ex