FIELD: metallurgy. SUBSTANCE: at the process of leaching at pH 4.5-3.0 sulfur (0.7-2.0 g / 1 g copper) is added to the pulp, and copper sulfide formed is separated by flotation. Sulfur particle size i 0.044-0.300 mm. Leaching involving sulfur addition is carried out at 50-95 C. EFFECT: simplified technology, decreased reagent consumption. 3 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING OF COBALT-BEARING MANGANESE-IRON CRUST FORMATIONS | 2004 |
|
RU2261923C1 |
METHOD OF IRON-MANGANESE CONCRETIONS REPROCESSING | 1986 |
|
SU1748450A1 |
METHOD OF FERROMANGANESE CONCRETION REPROCESSING | 1984 |
|
SU1665703A1 |
METHOD FOR FERRUM-MANGANESE GENERATION PROCESSING | 1990 |
|
SU1769543A1 |
METHOD OF PROCESSING UNDERWATER IRON-MANGANESE ORES | 2001 |
|
RU2184163C1 |
METHOD OF PROCESSING MANGANESE CONCRETIONS | 1998 |
|
RU2151813C1 |
UNDERWATER IRON-MANGANESE ORE PROCESSING METHOD | 2003 |
|
RU2231569C1 |
MANGANESE-CONTAINING ORE PROCESSING METHOD | 2000 |
|
RU2175022C1 |
METHOD FOR PROCESSING OF DIFFICULT-TO-OPEN SULFIDE PYRRHOTITE- CONTAINING MATERIALS PASSIVATED BY SULFIDE OXYGEN CORROSION PRODUCTS | 2002 |
|
RU2235139C1 |
METHOD OF PROCESSING OF HARD-FLOATABLE NICKEL-PYRRHOTINE MATERIALS BEARING NOBLE METALS | 2003 |
|
RU2249487C1 |
Authors
Dates
1994-04-30—Published
1984-08-24—Filed