FIELD: nuclear reactors. SUBSTANCE: temperature of collector is sustained to be no lower than 1000 K at loop reactor distortions of thermoemission assembly with tungsten emitters and collectors in vacuum degassing mode after thermal power is increased till level, at which temperature of emitter is equal to 1900-2000 K. EFFECT: improved efficiency.